Through our website / in-field consultations, We Provide a wide range of welding procedure specification which is conducted on Pipe lines, This Welding Procedure Specification had been done by multinational companies according to International standards and codes Like : BS 4515-1, DNV 2000, API 1104.

The scope of our WPS is to check the quality of the welded joints, guide welders to the accepted procedures so that repeatable and trusted welding techniques are used.

No. PQR No. Standard Base Metal P no. G no. Process Size Thickness Position  Filler metal Joint Type Heat Treatment 3rd Party Availabiolity
1 AAIS-WPS-PL-1 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 GTAW + SMAW 114.3mm to 323.9mm 12.5mm to 25mm All ER80S-G + E7018-G Single v N/A Velosi Upon Request
2 AAIS-WPS-PL-2 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 GTAW + SMAW 114.3mm to 323.9mm 12.5mm to 25mm All ER80S-G + E7018-G Single v N/A Velosi Upon Request
3 AAIS-WPS-PL-3 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 GTAW + SMAW 114.3mm to 323.9mm 12.5mm to 25mm All ER80S-G + E7018-G Single v N/A Velosi Upon Request
4 AAIS-WPS-PL-4 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 SMAW 114.3mm to 323.9mm 12.5mm to 25mm All E7018-G Single v N/A Velosi Upon Request
5 AAIS-WPS-PL-5 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 SMAW 114.3mm to 323.9mm 12.5mm to 25mm All E7018-G Single v N/A Velosi Upon Request
6 AAIS-WPS-PL-6 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 GTAW + SMAW 114.3mm to 323.9mm 12.5mm to 25mm All ER80S-G + E7018-G Single v N/A Velosi Upon Request
7 AAIS-WPS-PL-7 BS 4515-1 API 5L X60 / X 65 P 1 Gr 2 to P1 Gr 2 GTAW + SMAW 114.3mm to 323.9mm 12.5mm to 25mm All ER80S-G + E7018-G Single v N/A Velosi Upon Request
8 AAIS-WPS-PL-8 API 1104    API 5L Gr B P 1 Gr 1 to P1 Gr 1 SMAW 3-3/8" to 12-3/4 4.7mm to 19.05mm 5G E7010 + E7018 Single v N/A Germanisher lloyed Upon Request
9 AAIS-WPS-PL-9 API 1104    API 5L Gr B P 1 Gr 1 to P1 Gr 1 SMAW 2-3/8" to 12-3/4" 4.7mm to 19.05mm 6G E7010 + E7018 Single v N/A Germanisher lloyed Upon Request
10 AAIS-WPS-PL-10 API 1104    API 5L Gr B P 1 Gr 1 to P1 Gr 1 SMAW 2-3/8" to 12-3/4" 4.7mm to 19.05mm 6G E7010 + E7018 Single v N/A Germanisher lloyed Upon Request
11 AAIS-WPS-PL-11 API 1104    API 5L Gr B P 1 to P 1 SMAW 2-3/8" to 12-3/4" 4.7mm to 19.05mm 6G E7016 + E7018 Single v N/A Germanisher lloyed Upon Request
12 AAIS-WPS-PL-12 API 1104    API 5L X65 N/A SMAW 26" 19.1mm 5G E8010G Single v N/A   Upon Request
13 AAIS-WPS-PL-13 DNV2000  . API 5L X60 P 1 to P 1 SMAW 100mm to  300mm 5.3mm to 10.7mm 5G E8010G Single v N/A Bureau Veritas Upon Request
14 AAIS-WPS-PL-14 DNV2000  . API 5L X60 P 1 to P 1 SMAW 100mm to  300mm 5.3mm to 10.7mm 5G E7010G + E8010G Single v N/A Bureau Veritas Upon Request
15 AAIS-WPS-PL-15 API 1104   API 5L X60   SMAW 26" 19.1mm   E8010G Single v N/A Bureau Veritas Upon Request
16 AAIS-WPS-PL-16 API 1104   API 5L X60   SMAW 26" 19.1mm 5G E7016 + E 8018G Single v N/A Bureau Veritas Upon Request
17 AAIS-WPS-PL-17 API 1104   API 5L X60   SMAW 18" 17.5mm 5G E8010G Single v N/A Bureau Veritas Upon Request
18 AAIS-WPS-PL-18 API 1104    API 5L X65   SMAW 26" 19.1mm 5G E7016 + E8018G Single v N/A Bureau Veritas Upon Request
19 AAIS-WPS-PL-19 BS 4515    API 5L X60   SMAW 114.3mm to 323.9mm 12.5mm to 25mm All E8010-P1 Single v N/A Bureau Veritas Upon Request
20 AAIS-WPS-PL-20 BS 4515    API 5L X60 N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm All E8010-P1 Single v N/A Bureau Veritas Upon Request
21 AAIS-WPS-PL-21 BS 4515    API 5L X60 N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
22 AAIS-WPS-PL-22 BS 4515    API 5L X60 to ASTM A694 F60 N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
23 AAIS-WPS-PL-23 BS 4515    API 5L X60 to ASTM A694 F60 N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
24 AAIS-WPS-PL-24 BS 4515    ASTM 694 F65 to WPHY 65 SMLS N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
25 AAIS-WPS-PL-25 BS 4515    API 5L X65 N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
26 AAIS-WPS-PL-26 BS 4515    API 5L X65 N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm All E8010-P1 Single v N/A Bureau Veritas Upon Request
27 AAIS-WPS-PL-27 BS 4515    API 5L X65 to WPHY 65 SMLS N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
28 AAIS-WPS-PL-28 BS 4515    API 5L X60 to WPHY 65 SMLS N/A SMAW 114.3mm to 323.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
29 AAIS-WPS-PL-29 BS 4515    API 5L X65 to ASTM 694 F65 N/A SMAW > 325.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request
30 AAIS-WPS-PL-30 BS 4515    API 5L X65 to ASTM 694 F65 N/A SMAW > 325.9mm 12.5mm to 25mm 5G E8010-P1 Single v N/A Bureau Veritas Upon Request