A Welding Procedure Specification (WPS) is the formal written document describing welding procedures, which provides direction to the welder or welding operators for making sound and quality production welds as per the code requirements . Through our website / in-field consultations, We Provide a wide range of welding procedure specification which is conducted on Oil & Gas field Tanks, This Welding Procedure Specification had been done by multinational companies according to ASME IX, API 650 & API 653. The scope of our WPS is to check the quality of the welded joints, guide welders to the accepted procedures so that repeatable and trusted welding techniques are used. |
No. | PQR No. | Standard | Base Metal | P no. G no. | Process | Thickness | Position | Filler metal | Joint Type | Heat Treatment | 3rd Party |
1 | AAIS-WPS-T-1 | ASME IX | BS EN10025 S355 K2 or Eguivalent | P 1 Gr 2 to P 1 Gr 2 | SMAW | Up to 40mm | 3G | E 7018 | Double V | N/A | DNV.GL |
2 | AAIS-WPS-T-2 | ASME IX | BS EN10025 S355 K2 or Eguivalent | P 1 Gr 2 to P 1 Gr 2 | SMAW | Up to 40mm | 2G | E 7018 | Double Bevel | N/A | DNV.GL |
3 | AAIS-WPS-T-3 | ASME IX | S355JR / 182520-2 or Equivalent | P 1 Gr 1 to P 1 Gr 1 | GTAW + SMAW | Up to 30mm | 3G | ER 70S-6 + E7018-1 | Single V | N/A | DNV.GL |
4 | AAIS-WPS-T-4 | ASME IX | SA-516(70),UNS K02700 or Equivalent | P 1 Gr 2 to P 1 Gr 2 | GTAW + SMAW | Up to 40mm | 1G | ER 70S-6 + E7018-1 | Single V | Y | DNV.GL |
5 | AAIS-WPS-T-5 | ASME IX, API 653 & 650 | A 283 Gr c, A516 Gr 60,65 & 70 to JIS G3106 SM 520C(SM 53C MOD) | P 1 Gr 2 to P 1 Gr 2 | SMAW | 5mm to 25.4mm | 3G | E 7018 | Single V | N/A | DNV |
6 | AAIS-WPS-T-6 | ASME IX, API 653 & 650 | A 516 Gr 60,65 & 70 | P 1 Gr 2 to P 1 Gr 2 | SMAW | 12.7mm to 25.4mm | 3G | E 7018 | Single V | Yes | DNV |
7 | AAIS-WPS-T-7 | ASME IX | S275 JR / BS 4360 Gr 43C or Equivalent | N/A | SMAW | 4.8mm to 25mm | All | E 7018 | As attached | N/A | |
8 | AAIS-WPS-T-8 | ASME IX | S275 JR / BS 4360 Gr 43C or Equivalent | N/A | SMAW | 4.8mm to 25mm | All | E 7018 | As attached | N/A |